{"_buckets": {"deposit": "5d5055b7-4dc5-43af-91ef-9892f31cb5db"}, "_deposit": {"created_by": 2, "id": "14310", "owners": [2], "pid": {"revision_id": 0, "type": "depid", "value": "14310"}, "status": "published"}, "_oai": {"id": "oai:nagasaki-u.repo.nii.ac.jp:00014310", "sets": ["1200"]}, "author_link": ["51970", "51971", "51967", "51968", "51969", "51966"], "item_3_alternative_title_19": {"attribute_name": "その他のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "Effect of surface-oxidation treatment on the chemical stability of AIN powder"}]}, "item_3_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1989-01", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "32", "bibliographicPageEnd": "94", "bibliographicPageStart": "87", "bibliographicVolumeNumber": "19", "bibliographic_titles": [{"bibliographic_title": "長崎大学工学部研究報告"}, {"bibliographic_title": "Reports of the Faculty of Engineering, Nagasaki University", "bibliographic_titleLang": "en"}]}]}, "item_3_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Chemical stability toward water has been investigated for nine kinds of AIN powders which were prepared by two different processes. The powders prepared by reducing and nitriding alumina (A powders) exhibited more excellent chemical stabilities than those prepared by directly nitriding aluminum (B powders). The reason for these phenomena could be attributed to higher surface-activities of the B powders, because they included a large number of fine particles as well as fracture faces which were formed during the grinding process. The chemical stability was improved by surface-oxidation in nitrogen gas containing a trace amount of oxygen (below 5 ppm) at elevated temperatures, irrespective of the preparation method of AIN, though it was more effective for the A powders. The treatment of A powders at higher temperatures resulted in formation of a less amount of Al(OH)3 after dispersion in distilled water, that is in enhancement of chemical stability toward water. However, the treatment at higher temperatures also increased the oxygen content or α-Al2O3 on the surface. In view of high stability and low oxygen content, the treatment was most suitable at 1000℃ for 6 hr.", "subitem_description_type": "Abstract"}]}, "item_3_description_64": {"attribute_name": "引用", "attribute_value_mlt": [{"subitem_description": "長崎大学工学部研究報告, 19(32), pp.87-94; 1989", "subitem_description_type": "Other"}]}, "item_3_full_name_3": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "51969", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Shimizu, Yasuhiro"}]}, {"nameIdentifiers": [{"nameIdentifier": "51970", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Takatsuki, Seiji"}]}, {"nameIdentifiers": [{"nameIdentifier": "51971", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Egashira, Makoto"}]}]}, "item_3_publisher_33": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "長崎大学工学部"}]}, "item_3_source_id_10": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AN00178418", "subitem_source_identifier_type": "NCID"}]}, "item_3_source_id_7": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "02860902", "subitem_source_identifier_type": "ISSN"}]}, "item_3_source_id_8": {"attribute_name": "EISSN", "attribute_value_mlt": [{"subitem_source_identifier": "18805574", "subitem_source_identifier_type": "ISSN"}]}, "item_3_text_63": {"attribute_name": "出版者別言語", "attribute_value_mlt": [{"subitem_text_value": "Faculty of Engineering, Nagasaki University"}]}, "item_3_version_type_16": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "清水, 康博"}], "nameIdentifiers": [{"nameIdentifier": "51966", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "高月, 誠治"}], "nameIdentifiers": [{"nameIdentifier": "51967", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "江頭, 誠"}], "nameIdentifiers": [{"nameIdentifier": "51968", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2020-12-22"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "kogaku19_32_13.pdf", "filesize": [{"value": "2.8 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 2800000.0, "url": {"label": "kogaku19_32_13.pdf", "url": "https://nagasaki-u.repo.nii.ac.jp/record/14310/files/kogaku19_32_13.pdf"}, "version_id": "762c9474-5fb7-4af9-8b2a-85f53f3a5522"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "departmental bulletin paper", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "AIN粉体の化学的安定性に及ぼす表面酸化処理効果", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "AIN粉体の化学的安定性に及ぼす表面酸化処理効果"}]}, "item_type_id": "3", "owner": "2", "path": ["1200"], "permalink_uri": "http://hdl.handle.net/10069/24292", "pubdate": {"attribute_name": "公開日", "attribute_value": "2010-10-19"}, "publish_date": "2010-10-19", "publish_status": "0", "recid": "14310", "relation": {}, "relation_version_is_last": true, "title": ["AIN粉体の化学的安定性に及ぼす表面酸化処理効果"], "weko_shared_id": -1}
AIN粉体の化学的安定性に及ぼす表面酸化処理効果
http://hdl.handle.net/10069/24292
http://hdl.handle.net/10069/24292677e8986-830d-4ed8-bd98-bd6d6d923afa
名前 / ファイル | ライセンス | アクション |
---|---|---|
kogaku19_32_13.pdf (2.8 MB)
|
|
Item type | 紀要論文 / Departmental Bulletin Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2010-10-19 | |||||
タイトル | ||||||
タイトル | AIN粉体の化学的安定性に及ぼす表面酸化処理効果 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | departmental bulletin paper | |||||
著者 |
清水, 康博
× 清水, 康博× 高月, 誠治× 江頭, 誠 |
|||||
著者別名 | ||||||
姓名 | Shimizu, Yasuhiro | |||||
著者別名 | ||||||
姓名 | Takatsuki, Seiji | |||||
著者別名 | ||||||
姓名 | Egashira, Makoto | |||||
その他のタイトル | ||||||
その他のタイトル | Effect of surface-oxidation treatment on the chemical stability of AIN powder | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Chemical stability toward water has been investigated for nine kinds of AIN powders which were prepared by two different processes. The powders prepared by reducing and nitriding alumina (A powders) exhibited more excellent chemical stabilities than those prepared by directly nitriding aluminum (B powders). The reason for these phenomena could be attributed to higher surface-activities of the B powders, because they included a large number of fine particles as well as fracture faces which were formed during the grinding process. The chemical stability was improved by surface-oxidation in nitrogen gas containing a trace amount of oxygen (below 5 ppm) at elevated temperatures, irrespective of the preparation method of AIN, though it was more effective for the A powders. The treatment of A powders at higher temperatures resulted in formation of a less amount of Al(OH)3 after dispersion in distilled water, that is in enhancement of chemical stability toward water. However, the treatment at higher temperatures also increased the oxygen content or α-Al2O3 on the surface. In view of high stability and low oxygen content, the treatment was most suitable at 1000℃ for 6 hr. | |||||
書誌情報 |
長崎大学工学部研究報告 en : Reports of the Faculty of Engineering, Nagasaki University 巻 19, 号 32, p. 87-94, 発行日 1989-01 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 02860902 | |||||
EISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 18805574 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN00178418 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
出版者 | ||||||
出版者 | 長崎大学工学部 | |||||
出版者別言語 | ||||||
Faculty of Engineering, Nagasaki University | ||||||
引用 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 長崎大学工学部研究報告, 19(32), pp.87-94; 1989 |