{"_buckets": {"deposit": "7762a779-5246-4ddb-af42-3bcbbd4ef090"}, "_deposit": {"created_by": 2, "id": "8244", "owners": [2], "pid": {"revision_id": 0, "type": "depid", "value": "8244"}, "status": "published"}, "_oai": {"id": "oai:nagasaki-u.repo.nii.ac.jp:00008244", "sets": ["9"]}, "author_link": ["33716", "33714", "33715", "33713", "33717"], "item_2_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2012-10-02", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "5", "bibliographicPageEnd": "757", "bibliographicPageStart": "751", "bibliographicVolumeNumber": "31", "bibliographic_titles": [{"bibliographic_title": "Dental Materials Journal"}]}]}, "item_2_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "The purpose of this study was to evaluate the influence of air-abrasion and subsequent heat treatment on the shear bond strength of the bond between indirect composites and a zirconia material. Four surface preparations were employed; ground flat, then heated to regenerate the crystal phase (C); air-abraded with alumina for 10 s (S10), for 20 s (S20), and air-abraded for 10 s and heated (H). Disks were primed with Alloy Primer and bonded either with Estenia or with Gradia composite. XRD analysis suggested that the monoclinic zirconia content was increased by air-abrasion, and decreased by heating. The surface roughness of S10, S20 and H disks was similar. Nevertheless, H groups showed lower bond strengths than the S10 and S20 groups both before and after thermal cycling. Although alumina air-abrasion considerably enhanced bonding between zirconia and indirect composites, subsequent heat treatment had a negative effect on the durability of bond strength.", "subitem_description_type": "Abstract"}]}, "item_2_description_63": {"attribute_name": "引用", "attribute_value_mlt": [{"subitem_description": "Dental Materials Journal, 31(5), pp.751-757; 2012", "subitem_description_type": "Other"}]}, "item_2_publisher_33": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本歯科理工学会"}]}, "item_2_relation_12": {"attribute_name": "DOI", "attribute_value_mlt": [{"subitem_relation_type": "isIdenticalTo", "subitem_relation_type_id": {"subitem_relation_type_id_text": "10.4012/dmj.2012-077", "subitem_relation_type_select": "DOI"}}]}, "item_2_rights_13": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "© 2012 The Japanese Society for Dental Materials and Devices"}]}, "item_2_source_id_7": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "02874547", "subitem_source_identifier_type": "ISSN"}]}, "item_2_source_id_8": {"attribute_name": "EISSN", "attribute_value_mlt": [{"subitem_source_identifier": "18811361", "subitem_source_identifier_type": "ISSN"}]}, "item_2_text_62": {"attribute_name": "出版者別言語", "attribute_value_mlt": [{"subitem_text_value": "The Japanese Society for Dental Materials and Devices"}]}, "item_2_version_type_16": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "Shimoe, Saiji"}], "nameIdentifiers": [{"nameIdentifier": "33713", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Tanoue, Naomi"}], "nameIdentifiers": [{"nameIdentifier": "33714", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Kusano, Kenta"}], "nameIdentifiers": [{"nameIdentifier": "33715", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Okazaki, Masayuki"}], "nameIdentifiers": [{"nameIdentifier": "33716", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Satoda, Takahiro"}], "nameIdentifiers": [{"nameIdentifier": "33717", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2020-12-21"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "DMJ31_751.pdf", "filesize": [{"value": "1.9 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 1900000.0, "url": {"label": "DMJ31_751.pdf", "url": "https://nagasaki-u.repo.nii.ac.jp/record/8244/files/DMJ31_751.pdf"}, "version_id": "4cb0c6a3-6c8f-4cf1-a011-836d520c7be8"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Air-abrasion", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Bond strength", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Heat treatment", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Indirect composite", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Zirconia", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "eng"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "Influence of air-abrasion and subsequent heat treatment on bonding between zirconia framework material and indirect composites", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "Influence of air-abrasion and subsequent heat treatment on bonding between zirconia framework material and indirect composites"}]}, "item_type_id": "2", "owner": "2", "path": ["9"], "permalink_uri": "http://hdl.handle.net/10069/30986", "pubdate": {"attribute_name": "公開日", "attribute_value": "2013-03-13"}, "publish_date": "2013-03-13", "publish_status": "0", "recid": "8244", "relation": {}, "relation_version_is_last": true, "title": ["Influence of air-abrasion and subsequent heat treatment on bonding between zirconia framework material and indirect composites"], "weko_shared_id": -1}
Influence of air-abrasion and subsequent heat treatment on bonding between zirconia framework material and indirect composites
http://hdl.handle.net/10069/30986
http://hdl.handle.net/10069/30986c95afb22-43e0-4818-a656-e0ea304e7e9f
名前 / ファイル | ライセンス | アクション |
---|---|---|
DMJ31_751.pdf (1.9 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2013-03-13 | |||||
タイトル | ||||||
タイトル | Influence of air-abrasion and subsequent heat treatment on bonding between zirconia framework material and indirect composites | |||||
言語 | ||||||
言語 | eng | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Air-abrasion | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Bond strength | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Heat treatment | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Indirect composite | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Zirconia | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
著者 |
Shimoe, Saiji
× Shimoe, Saiji× Tanoue, Naomi× Kusano, Kenta× Okazaki, Masayuki× Satoda, Takahiro |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | The purpose of this study was to evaluate the influence of air-abrasion and subsequent heat treatment on the shear bond strength of the bond between indirect composites and a zirconia material. Four surface preparations were employed; ground flat, then heated to regenerate the crystal phase (C); air-abraded with alumina for 10 s (S10), for 20 s (S20), and air-abraded for 10 s and heated (H). Disks were primed with Alloy Primer and bonded either with Estenia or with Gradia composite. XRD analysis suggested that the monoclinic zirconia content was increased by air-abrasion, and decreased by heating. The surface roughness of S10, S20 and H disks was similar. Nevertheless, H groups showed lower bond strengths than the S10 and S20 groups both before and after thermal cycling. Although alumina air-abrasion considerably enhanced bonding between zirconia and indirect composites, subsequent heat treatment had a negative effect on the durability of bond strength. | |||||
書誌情報 |
Dental Materials Journal 巻 31, 号 5, p. 751-757, 発行日 2012-10-02 |
|||||
出版者 | ||||||
出版者 | 日本歯科理工学会 | |||||
出版者別言語 | ||||||
The Japanese Society for Dental Materials and Devices | ||||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 02874547 | |||||
EISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 18811361 | |||||
DOI | ||||||
関連タイプ | isIdenticalTo | |||||
識別子タイプ | DOI | |||||
関連識別子 | 10.4012/dmj.2012-077 | |||||
権利 | ||||||
権利情報 | © 2012 The Japanese Society for Dental Materials and Devices | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
引用 | ||||||
内容記述タイプ | Other | |||||
内容記述 | Dental Materials Journal, 31(5), pp.751-757; 2012 |