@article{oai:nagasaki-u.repo.nii.ac.jp:00014237, author = {内田, 武 and 高瀬, 徹 and 楠本, 韶 and 梶, 聖悟}, issue = {27}, journal = {長崎大学工学部研究報告, Reports of the Faculty of Engineering, Nagasaki University}, month = {Jul}, note = {Fracture toughness of single crystal ice was investigated using sharply edge-notched specimens by three point bending at -10℃. The loading rate K1 was about 200 kPa・m1/2/s. The notch of the specimens was made by pressing the edge of a razor blade on the bottom of the saw cut slot. Four types of specimen were used, in which C-axis of the crystal was placed at an angle 0°, 45°(I), 45 °(II), 90 ° respectively to the notch plane. Observation on the patterns of fracture surface relating to the angle θ and y is also described., 長崎大学工学部研究報告, 16(27), pp.107-112; 1986}, pages = {107--112}, title = {単結晶氷の破壊じん性およびマクロフラクトグラフィ}, volume = {16}, year = {1986} }