@article{oai:nagasaki-u.repo.nii.ac.jp:00016062, author = {Nakano, Masaki and Sato, S. and Fukunaga, Hirotoshi and Yamashita, F.}, issue = {8}, journal = {Journal of Applied Physics}, month = {Apr}, note = {The interceptive deposition method (IDM) was applied to the high-speed pulsed laser deposition (PLD) method with a substrate heating system, and it was clarified that anisotropic Nd-Fe-B thick-film magnets can be obtained under a high deposition rate larger than 20-50 μm/h. The obtained coercivity, remanence, and (BH)max values of a film were 577 kA/m, 0.90 T, and 118 kJ/m3, respectively. In addition, we succeeded in increasing the thickness up to 90 μm for an anisotropic Nd-Fe-B film magnet by using IDM. c2006 American Institute of Physics, Journal of Applied Physics, 99(8), 08N301; 2006}, pages = {08N301-1--08N301-3}, title = {A method of preparing anisotropic Nd-Fe-B film magnets by pulsed laser deposition.}, volume = {99}, year = {2006} }